Classification: Low Expansion Alloy
Density: 8.19
Resisivity: 0.55
Curie Point: 400
State: Soft
Brand: 4j47
Customization:
Diamond Member Since 2016

Suppliers with verified business licenses

Rating: 5.0/5
Manufacturer/Factory

Basic Info.

Model NO.
Kovar
Chemical Composition
Feni47cr
OEM
Yes
Sample
Free
Stock
Seyn
Material
Fe- Ni Alloy
Surface
Smooth and Bright
Condition
Soft
Magnetic Properties
Less Than 230 Celsius Is Ferromagnetic.
Heat Treatment
Done
Thickness
0.1-2mm
Transport Package
Export Packing
Specification
Can discuss
Trademark
HUONA
Origin
Shanghai
HS Code
722699900
Production Capacity
300 Tons / Month

Product Description


4J29 FeNi Kovar Expension Alloy Strip

Classification : the alloy of expansion characteristics

Application: Kovar (trademark of CRS Holdings, inc., Delaware[1]) is a nickel-cobalt ferrous alloy compositionally identical to Fernico 1, designed to be compatible with the thermal expansion characteristics of borosilicate glass (~5 × 10?6 /K between 30 and 200 °C, to ~10 × 10?6 /K at 800 °C) in order to allow direct mechanical connections over a range of temperatures. It finds application in electroplated conductors entering glass envelopes of electronic parts such as vacuum tubes (valves), X-ray and microwave tubes and some lightbulbs.
  
Chemical Composition in %  Kovar


 Ni
28,5-29,5%

Fe
51,14-54,5%

C
0.03%

Si
0.3%

Mn
0,4 %

S
o 0.015%

P
0.015%

o
17-18%

Ti
0.1%

Al
0.2%

Cu
0.2%

Cr
0,1 %
 
 The thermal properties of alloy
 
Temperature coefficient of linear expansion αsr ? 10-6 K-1 in the temperature range, ° C inflection point temperature, ° C
No less
Heat treatment regime blanks and samples
20-80 20-100 20-300 20-400 20-450 20-500 20-800
- - 4,6-5,6 4,6-5,2 - 5,9-6,4 - 420 samples and blanks annealing in hydrogen, a vacuum or protective atmosphere at a temperature (960 ± 20) ° C, holding 1 hr., cooling with the furnace or container to 200 ° C at a rate not exceeding 10 ° C / min
Property sintered HIPed
Density / g cm3 8.0 8.35
Hardness / HV1 160 150
Youngs Modulus / GPa 138 138
reduction of area at fracture / % 30 30
yield strength / MPa 270 270
thermal conductivity / W/Km 17
Curie Temperature / °C 435
electrical resistivity Ω mm2 / m 0.49
specific heat J/gK 0.46
thermal expansion coefficient/10?6 K?1 (25 - 200 °C) 5.5
(25-300 °C) 5.1
(25-400 °C) 4.9
(25-450 °C) 5.3
(25-500 °C) 6.2

4J29 FeNi Kovar Expension Alloy Strip

The name Kovar is often used as a general term for Fe-Ni alloys with these particular thermal expansion properties. Note the related particular Fe-Ni alloy Invar which exhibits minimum thermal expansion.
 
We referring to the presence of high-power production, offers customers buy alloy Kovar in the required quantities and ensures minimum time shipments of rolled metal products, made on the basis of Kovar.

4j29 Feni Kovar Expension Alloy Strip
 

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now