Customization: | Available |
---|---|
Insulation Level: | C, H, F, B, E |
Certification: | ISO9001, RoHS |
Still deciding? Get samples of US$ 50/kg
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Product Description
These enameled resistance wires have been broadly used for standard resistors, automobile
parts, winding resistors, etc. using the insulation processing best suited for these applications, taking full advantage of the distinctive features of enamel coating.
Furthermore, we will carry out enamel coating insulation of precious metal wire such as silver and platinum wire upon order. Please make use of this production-on-order.
Tpye of Insulation:
1) Polyester resistance wire , class 130
2) Modified polyester resistance wire , class 155
3) Polyesterimide resistance wire , class 180
4) Polyester (imide) coated with polyamide-imide resistance wire , class 200
5) Polyimide resistance wire , class 220
Constantan 6J40 | New Constantan | Manganin | Manganin | Manganin | ||
6J11 | 6J12 | 6J8 | 6J13 | |||
Main Chemical Elements % | Mn | 1~2 | 10.5~12.5 | 11~13 | 8~10 | 11~13 |
Ni | 39~41 | - | 2~3 | - | 2~5 | |
Cu | REST | REST | REST | REST | REST | |
Al2.5~4.5 Fe1.0~1.6 | Si1~2 | |||||
Temperature Range for Components | 5~500 | 5~500 | 5~45 | 10~80 | 10~80 | |
Density | 8.88 | 8 | 8.44 | 8.7 | 8.4 | |
g/cm3 | ||||||
Resistivity | 0.48 | 0.49 | 0.47 | 0.35 | 0.44 | |
μΩ.m,20 | ±0.03 | ±0.03 | ±0.03 | ±0.05 | ±0.04 | |
Extensibility | ≥15 | ≥15 | ≥15 | ≥15 | ≥15 | |
%Φ0.5 | ||||||
Resistance | -40~+40 | -80~+80 | -3~+20 | -5~+10 | 0~+40 | |
Temperature | ||||||
Quotiety | ||||||
α,10 -6 / | ||||||
Thermoelectromotive | 45 | 2 | 1 | 2 | 2 | |
force to Copper | ||||||
μv/(0~100) |
Tpye of Bare Wire
main property type |
|
Cuni1 |
CuNI2 |
CuNI6 |
CuNI10 |
CuNi19 |
CuNi23 |
CuNi30 |
CuNi34 |
CuNI44 |
main chemical composition |
Ni |
1 |
2 |
6 |
10 |
19 |
23 |
30 |
34 |
44 |
|
MN |
/ |
/ |
/ |
/ |
0.5 |
0.5 |
1.0 |
1.0 |
1.0 |
|
CU |
rest |
rest |
rest |
rest |
rest |
rest |
rest |
rest |
rest |
max working temperature |
|
/ |
200 |
220 |
250 |
300 |
300 |
350 |
350 |
400 |
density g/cm3 |
|
8.9 |
8.9 |
8.9 |
8.9 |
8.9 |
8.9 |
8.9 |
8.9 |
8.9 |
resistivity at 20 °c |
|
0.03 |
0.05 |
0.1 |
0.15 |
0.25 |
0.3 |
0.35 |
0.40 |
0.49 |
temperature coefficient of resistance |
|
<100 |
<120 |
<60 |
<50 |
<25 |
<16 |
<10 |
-0 |
<-6 |
tensile strength mpa |
|
>210 |
>220 |
>250 |
>290 |
>340 |
>350 |
>400 |
>400 |
>420 |
elongation |
|
>25 |
>25 |
>25 |
>25 |
>25 |
>25 |
>25 |
>25 |
>25 |
melting point °c |
|
1085 |
1090 |
1095 |
1100 |
1135 |
1150 |
1170 |
1180 |
1280 |
coefficient of conductivity |
|
145 |
130 |
92 |
59 |
38 |
33 |
27 |
25 |
23 |